Part 28 (1/2)
Must be contained in water-proof case (stout paper), water-proofed with Resin and Cerasin--No 6 detonator
~Withnell Powder~
Ammonium Nitrate 88-92 parts
Tri-nitro-Toluene 4-6 ”
Flour (dried at 100 C) 4-6 ”
Moisture 0-15 ”
Only to be used when contained in a linen paper cartridge, water-proofed with Carnuba Wax, Parrafin--No 7 detonator used
~Phenix Powder~
Nitro-Glycerine 28-31 parts
Nitro-Cotton 0-1 ”
Potassium Nitrate 30-34 ”
Wood Meal 33-37 ”
Moisture 2-6 ”
~SMOKELESS POWDERS~
~Cordite~
Nitro-Glycerine 58 per cent +or- 75 Nitro-Cotton 37 ” +or- 65 Vaseline 5 ” +or- 25
~Cordite, MD~
Nitro-Glycerine 30 per cent +or- 1 Nitro-Cotton 65 ” +or- 1 Vaseline 5 ” +or- 25
analysis of-- By W Mancab and AE Leighton
~EC Powder~
Nitro-Cotton 790 per cent
Potassium Nitrate 45 ”
Barium Nitrate 75 ”
Camphor 41 ”
Wood Meal 38 ”
Volatile Matter 11 ”
~Walarode Powder~
Nitro-Cotton 986 per cent
Volatile Matter 14 ”
~Kynoch's Smokeless~
Nitro-Cotton 521 per cent
Di-nitro-Toluene 195 ”
Potassium Nitrate 14 ”
Barium Nitrate 222 ”
Wood Meal 27 ”
Ash 09 ”